Ụlọ ọrụ Sintered SmCoIgwe ỌdụdọNjirimara anụ ahụ | |||||||||
Ihe onwunwe | Ọkwa | Ịnọgide | Rev. Temp.- Coeff. Nke Br | Ike mmanye | Ike mmanye n'ime ime | Rev. Temp.-Coeff. Nke Hcj | Oke. Ngwaahịa ike | Oke. Okpomọkụ na-arụ ọrụ | Njupụta |
Br (KGs) | Hcb (Ị) | Hcj (Ị) | (BH) kacha. (MGOe) | g/cm³ | |||||
SmCo5 | XG16 | 8.1-8.5 | -0.050 | 7.8-8.3 | 15-23 | -0.30 | 14-16 | 250 ℃ | 8.3 |
XG18 | 8.5-9.0 | -0.050 | 8.3-8.8 | 15-23 | -0.30 | 16-18 | 250 ℃ | 8.3 | |
XG20 | 9.0-9.4 | -0.050 | 8.5-9.1 | 15-23 | -0.30 | 19-21 | 250 ℃ | 8.3 | |
XG22 | 9.2-9.6 | -0.050 | 8.9-9.4 | 15-23 | -0.30 | 20-22 | 250 ℃ | 8.3 | |
XG24 | 9.6-10.0 | -0.050 | 9.2-9.7 | 15-23 | -0.30 | 22-24 | 250 ℃ | 8.3 | |
XG16S | 7.9-8.4 | -0.050 | 7.7-8.3 | ≥23 | -0.28 | 15-17 | 250 ℃ | 8.3 | |
XG18S | 8.4-8.9 | -0.050 | 8.1-8.7 | ≥23 | -0.28 | 17-19 | 250 ℃ | 8.3 | |
XG20S | 8.9-9.3 | -0.050 | 8.6-9.2 | ≥23 | -0.28 | 19-21 | 250 ℃ | 8.3 | |
XG22S | 9.2-9.6 | -0.050 | 8.9-9.5 | ≥23 | -0.28 | 21-23 | 250 ℃ | 8.3 | |
XG24S | 9.6-10.0 | -0.050 | 9.3-9.9 | ≥23 | -0.28 | 23-25 | 250 ℃ | 8.3 | |
Sm2Co17 | XG24H | 9.5-10.2 | -0.025 | 8.7-9.6 | ≥25 | -0.20 | 22-24 | 350 ℃ | 8.3 |
XG26H | 10.2-10.5 | -0.030 | 9.4-10.0 | ≥25 | -0.20 | 24-26 | 350 ℃ | 8.3 | |
XG28H | 10.3-10.8 | -0.035 | 9.5-10.2 | ≥25 | -0.20 | 26-28 | 350 ℃ | 8.3 | |
XG30H | 10.8-11.0 | -0.035 | 9.9-10.5 | ≥25 | -0.20 | 28-30 | 350 ℃ | 8.3 | |
XG32H | 11.0-11.3 | -0.035 | 10.2-10.8 | ≥25 | -0.20 | 29-32 | 350 ℃ | 8.3 | |
XG22 | 9.3-9.7 | -0.020 | 8.5-9.3 | ≥18 | -0.20 | 20-23 | 300 ℃ | 8.3 | |
XG24 | 9.5-10.2 | -0.025 | 8.7-9.6 | ≥18 | -0.20 | 22-24 | 300 ℃ | 8.3 | |
XG26 | 10.2-10.5 | -0.030 | 9.4-10.0 | ≥18 | -0.20 | 24-26 | 300 ℃ | 8.3 | |
XG28 | 10.3-10.8 | -0.035 | 9.5-10.2 | ≥18 | -0.20 | 26-28 | 300 ℃ | 8.3 | |
XG30 | 10.8-11.0 | -0.035 | 9.9-10.5 | ≥18 | -0.20 | 28-30 | 300 ℃ | 8.3 | |
XG32 | 11.0-11.3 | -0.035 | 10.2-10.8 | ≥18 | -0.20 | 29-32 | 300 ℃ | 8.3 | |
XG26M | 10.2-10.5 | -0.035 | 8.5-9.8 | 12-18 | -0.20 | 24-26 | 300 ℃ | 8.3 | |
XG28M | 10.3-10.8 | -0.035 | 8.5-10.0 | 12-18 | -0.20 | 26-28 | 300 ℃ | 8.3 | |
XG30M | 10.8-11.0 | -0.035 | 8.5-10.5 | 12-18 | -0.20 | 28-30 | 300 ℃ | 8.3 | |
XG32M | 11.0-11.3 | -0.035 | 8.5-10.7 | 12-18 | -0.20 | 29-32 | 300 ℃ | 8.3 | |
XG24L | 9.5-10.2 | -0.025 | 6.8-9.0 | 8-12 | -0.20 | 22-24 | 250 ℃ | 8.3 | |
XG26L | 10.2-10.5 | -0.035 | 6.8-9.4 | 8-12 | -0.20 | 24-26 | 250 ℃ | 8.3 | |
XG28L | 10.3-10.8 | -0.035 | 6.8-9.6 | 8-12 | -0.20 | 26-28 | 250 ℃ | 8.3 | |
XG30L | 10.8-11.5 | -0.035 | 6.8-10.0 | 8-12 | -0.20 | 28-30 | 250 ℃ | 8.3 | |
XG32L | 11.0-11.5 | -0.035 | 6.8-10.2 | 8-12 | -0.20 | 29-32 | 250 ℃ | 8.3 | |
Mara: · Anyị na-anọgide otu dị ka n'elu ma ọ bụrụ na kpọmkwem si ahịa. Curie okpomọkụ na ọnụọgụ okpomọkụ bụ naanị maka ntụnye aka, ọ bụghị dị ka ihe ndabere maka mkpebi.· Oke okpomọkụ na-arụ ọrụ nke magnet na-agbanwe n'ihi oke ogologo na dayameta na ihe gburugburu ebe obibi. |
Uru:
A na-edozi iji magnetik ndị a site na okpomọkụ dị n'ọtụtụ dị iche iche na-agba ọsọ site na 250ºC ruo 350ºC na okpomọkụ Curie ha nwere ike ịdị elu.
dị ka 710 ruo 880 Celsius. Ya mere, SmCo magnet nwere mma magnetik kwụsie ike n'ihi na elu iguzogide elu okpomọkụ.
A na-eji ihe ndọta SmCo mara oke nguzogide corrosion, enweghị mkpuchi achọrọ maka nchekwa elu.
Njirimara:
Mwepu nke magnetik SmCo bụ njiri mara nke ihe - ihe na-aghaghị iburu n'uche n'oge nhazi.
A na-eji galvanized ma ọ bụ kpuchie ihe ndọta ahụ site na electrodeposition cathodic maka ụfọdụ ngwa.
Ngwa:
N'ebe okpomọkụ dị elu na-arụ ọrụ, nnukwu corrosion na oxidation resistance dị oke mkpa. Dị ka, eletrọnịkị magnetron,Igwe Ọdụdọnnyefe ic,
Ọgwụgwọ magnetik, Magnistor, wdg.
Ekpebiri ụkpụrụ niile ekwuru site na iji nlele ọkọlọtọ dịka IEC 60404-5. Nkọwa ndị a na-eje ozi dị ka ụkpụrụ ntụnye aka na ike
iche. Nke kacha. Ọnọdụ okpomọkụ na-arụ ọrụ dabere na akụkụ magnet na ngwa akọwapụtara. Maka ozi ndị ọzọ biko kpọtụrụ anyị